Description
This equioment is mainly used for lithiumĀ battery electrode coateing
In the production process slurry drying process.
Transferring Speed: 1m/min continuously adjustable:
Oven temperature: room temperature ~ 150 degree C adjustable;
Electrode width: <- 300mm;
Coated precision: <- + – 0.003mm
Coating method: single row;
Heating zone: 1 zone; Dimensions: L*W*H = 1800* 800*1200;